Modified Guideline for Use of Reinforcement Steel in RCC Structures
Authority/ Engineer in Charge of the works are also advised to check the quality of the HSD bars undergone through heat treatment (Quenching and self-tempering) by doing the Ring test with Nital (5% nitric acid in alcohol).